I've been doing some sluicing testing and have achieved the following overall results: | I've been doing some sluicing testing and have achieved the following overall results: | ||
:1, | :1,400 gravel processed into ores: 346 copper (~25%), 349 tin (~25%), 275 coal (~20%), 290 iron (~20%), 88 gold (~6%), 27 titanium (~2%), 25 platinum (~2%). Last updated: --[[User:McClaw|McClaw]] ([[User talk:McClaw|talk]]) 07:39, 10 June 2015 (MDT) |