I've been doing some sluicing (looking for titanium) and have achieved the following:
I've been doing some sluicing testing and have achieved the following overall results:
:400 gravel processed into ores: 102 copper (25.5%), 90 tin (22.5%), 83 coal (20.75%), 83 iron (20.75%), 28 gold (7%), 8 titanium (2%), 6 platinum (1.5%). --[[User:McClaw|McClaw]] ([[User talk:McClaw|talk]]) 15:12, 28 November 2014 (MST)
:500 gravel processed into ores: 121 copper (24.2%), 116 tin (23.2%), 106 coal (21.2%), 105 iron (21.0%), 33 gold (6.6%), 10 titanium (2%), 9 platinum (1.8%). --[[User:McClaw|McClaw]] ([[User talk:McClaw|talk]]) 14:44, 1 December 2014 (MST)

Revision as of 17:44, 1 December 2014

Trial Results

I've been doing some sluicing testing and have achieved the following overall results:

500 gravel processed into ores: 121 copper (24.2%), 116 tin (23.2%), 106 coal (21.2%), 105 iron (21.0%), 33 gold (6.6%), 10 titanium (2%), 9 platinum (1.8%). --McClaw (talk) 14:44, 1 December 2014 (MST)